Water-based coolant is made of high purity water and highly efficient compound corrosion inhibitor. agent, etc. It is a pre-diluted coolant This product is a pre-diluted coolant and can be used directly. (This product can also be prepared as a concentrate).
Features and Usages
• Excellent thermal conductivity for long-lasting thermostatic protection;
• Excellent metal corrosion protection and non-metallic compatibility, extending the life of the data centre's cooling and heat exchange circulation system;
• Long life cycle, long time protection of data centre coolant and heat exchanger circulatory system, reducing data centre maintenance costs;
• Non-toxic to human body and biology, environmentally friendly;
• Meet the requirements of EU RoHS, REACH and other regulations.
|
PROJECT
|
TYPICAL DATA
|
TEST METHOD
|
||
|
Odour
|
No irritating odour
|
Olfactor
|
||
|
Color
|
Red
|
Visual estimation
|
||
|
Density(20.0℃)/(g/cm^3)
|
1.000
|
SH/T 0068
|
||
|
Freezing point/℃
|
0.0 |
SH/T 0090
|
||
|
Boiling point/℃
|
100.0 |
SH/T 0089
|
||
|
Ash content(Mass fraction)/%
|
0.33 |
SH/T 0067
|
||
|
pH value
|
8.5 |
SH/T 0069
|
||
|
Chlorine content/(mg/kg)
|
2 |
SH/T 0621
|
||
|
Reserve alkalinity/ml
|
2.4 |
SH/T 0091
|
||
|
Effect on organic coatings
|
No effect
|
SH/T 0084
|
||
|
Corrosion of
glassware
(88℃±2℃,
336h±2h)
|
Change
in mass
(mg/Test
piece)
|
Purple copper
|
1.1 |
SH/T 0085
|
|
Brass
|
0.9 | |||
|
Steel
|
1.0 | |||
|
Cast iron
|
1.1 | |||
|
Solder
|
2.3 | |||
|
Cast aluminium
|
1.3 | |||
|
Corrosion of
glassware
(88℃±2℃,
1064h±2h)
|
Change
in mass
(mg/Test
piece)
|
Purple copper
|
2.0 |
SH/T 0085
|
|
Brass
|
2.1 | |||
|
Steel
|
1.4 | |||
|
Cast iron
|
1.7 | |||
|
Solder
|
2.6 | |||
|
Cast aluminium
|
2.3 | |||
|
Bubble tendency
(70 ±1℃)
|
Foam volume/ml
|
35 |
SH/T 0066
|
|
|
Foam disappearance time/s
|
1.0 | |||
|
Heat transfer corrosion of aluminium alloy (135℃±1℃, 168h±2h)Mass change rate/(mg/cm2)
|
0.3 |
SH/T 0620
|
||
Note: Customized products for other working conditions are available.
Suitable for cooling and heat exchange circulation systems in data centres without frost protection requirements.
anterior:Two-Phase Dielectric Fluid
próximo:ninguno
Related Product
+Newsmore
- 01 Feb,2024Dry Cooler D4-8x910 In Stock Is On Sale! Discount!
- 06 Sep,2023Pad Adiabatic Dry Cooler Trial Operation Before Shipment
- 06 Sep,2023828kW Adiabatic Cooling System Dry Cooler Loading
- 17 Aug,2022Flat Type Dry Cooler Finished For Canada Client
- 06 Sep,20231061kW dry cooler loading for USA client
- 31 Mar,2021Peru client Install Shenglin Adiabatic Dry Cooler At Site